Abstract

Ni44.1Mn44.2Sn11.7 ribbons were prepared by melt spinning. After heat treatment, the martensitic transformation (MT) temperature increases obviously in the annealed ribbons. Large magnetoresistance (MR) was observed in these ribbons. Under the field of 50 kOe, the maximum values of negative MR were 22% for melt-spun ribbons at 240 K and 38% for annealed ribbons at 268 K, respectively. The annealing effect on MT and MR, together with the origin of the large MR, has been discussed in this paper.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.