Abstract
Composite PM 6061 aluminium alloy based metal matrix composites were manufactured by wet blending of 6061 alloy powder and δ alumina Saffil fibres followed by hot direct extrusion of the powder-fibre blends in closed containers through a streamline die, then heat treated to T6 condition (solution treated at 540°C for 5 h and age hardened at 160°C for 16 h). Density depended on the reinforcement content: relative densities of 97.5% for composite material containing 30 vol.-% fibres to 99.3% for composite material with 10 vol.-% fibres were obtained
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.