Abstract

Hydroxyapatite [HAp; Ca 10(PO 4) 6(OH) 2] biocomposites are ceramic materials that exhibit excellent bioactivity, but their inherent low fracture strength and toughness render them unusable for practical applications. Alumina (Al 2O 3) is added to improve in mechanical properties without diminution of biocompatibility. Powder mixtures of HAp and Al 2O 3 in various volume ratios (90:10, 80:20, and 70:30) were compacted by underwater shock waves generated by explosives. High explosives of 6900 m s −1 detonation velocity served as the energy generators. The compacts were sintered at 1473, 1573, and 1673 K in order to investigate the influence of sintering temperature. All compacts were found to be free of defects and to have undergone continuous compositional changes to α tricalcium phosphate and tetracalcium phosphate. K 1c showed maximum value with HAp–30vol.% Al 2O 3 that have been sintered at 1673 K for 7.2 ks, and the value of 3.0 MPa m −1/2 is 2.5 times that of HAp monolithic material. The results of optical microscopy, scanning electron microscopy, X-ray diffraction, and other analyses are reported.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.