Abstract

Abstract The addition of Pt prolongs the lifetime of the PdO/Al2O3 catalyst during CH4 combustion at 1073 K. Furthermore, the addition of ZrO2, La2O3 and Nd2O3 greatly extends the lifetime of the Pt–PdO/Al2O3 catalyst. This is due not to the transformation of PdO to Pd–Pt but to the prevention of the growth of PdO particles during the reaction.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.