Abstract

The present study was conducted to evaluate the effect of acidic primers on adhesive bonding to sintered alumina. Alumina disk specimens were primed with one of the following acidic materials: Acryl Bond, All Bond II Primer B, Alloy Primer, Estenia Opaque Primer, Eye Sight Opaque Primer, M.L. Primer, MR. Bond, and Super-Bond Liquid. The disks were bonded with an adhesive resin (Super-Bond) initiated with a tri-n-butylborane (TBB) derivative, and bond strengths were determined. Average bond strength before thermocycling varied from 42.9 to 44.3 MPa, whereas post-thermocycling bond strength ranged from 22.0 to 42.8 MPa. Of the nine groups assessed, reduction of bond strength after thermocycling was not significant in three: Alloy Primer, Estenia Opaque Primer, and Eye Sight Opaque Primer. It can be concluded that phosphate-based primers are recommended for bonding sintered alumina with Super-Bond resin.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.