Research on the effect of acid treatment on the opening of the pore mouths on the surface of the zeolite catalyst has been carried out. The preparation of the zeolite catalyst was carried out through the processes of soaking, calcination, oxidation and reduction. Initially, the zeolite was soaked for 3 hours in distilled water, then drained and crushed until its size passed a 100 mesh sieve, followed by a calcination process with nitrogen for 5 hours. Then proceed with oxidation for 3 hours followed by a reduction process for 2 hours with hydrogen. Furthermore, the catalyst was impregnated with Ni from the salt Ni.(NO3).6H2O After that the catalyst is stored and placed in a desiccator. Then an analysis of the catalyst obtained with AAS was carried out to determine the content of Na, Ca, Fe, Mg and K cations, and the content of Al and Si. Then continued with the analysis of acidity with gravimetric method and continued with analysis with the BET method to determine the specific surface area and pore size distribution. Furthermore, the catalyst is used in the catalytic cracking process at various temperatures.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.