Abstract
A study on the individual role of γ and γ′-phase during the scale formation on Co-9Al-9W (at.%) at 900 °C was conducted. High-accuracy thermogravimetric analysis was used to locate changes in the kinetics of scale growth. Compositions of three separated layers within the scale have been elucidated in detail. The results demonstrate the substantial impact of the two-phase microstructure on the initiation of oxidation for the appearance of the scale. Examination of STEM-EDX elemental mappings of the internal oxidation front during the early stages of scale growth can explain the origin of isolated Al2O3 precipitates instead of a closed protective layer.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.