Abstract
In this study, to characterize the high-rate tensile properties of a Nickel-base single crystal superalloy at high temperatures, an improved technique for conducting split Hopkinson tensile bar (SHTB) tests at high temperatures (up to 1200°C) is developed. A Quick Hook Joint method to rapidly mount the specimen to the SHTB system is adopted in the technique. Firstly, the specimen is heated to target temperature while keeping the bars at the room temperature. Then the Quick Hook Joint method is used to quickly assemble the specimen to the SHTB by a synchronically dual-actuator assembled system, immediately before loading is imposed to the specimen. The cold contact time (CCT) experienced by the specimen is measured by laser sensors and the cold contact process is numerically simulated. The results show that no evident temperature decrease in the specimen gauge section and no significant temperature increase in the loading bars. Finally, tensile experiments of a single-crystal Nickel-base superalloy over a temperature range of 298–1473K and over a strain-rate range of 0.001–3000s−1 are conducted. Anomalous high temperature peak of flow stress is noticed in the experimental results, and the peak of the flow stress shifts to higher temperature as the strain rate increases. Anomalous temperature valley of the fracture strain is formed over the selected temperature range, and the valley of the fracture strain also shifts to higher temperature as the strain rate increases. A model is applied to quantitatively describe the strain-rate effect on the anomalous peak of the flow stress over a wide range of strain rates.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.