Abstract

Quasi-static and high-rate tensile experiments were used to examine the strain rate sensitivity of laser-directed energy deposition (L-DED)- and additive friction stir deposition (AFSD)-formed AerMet 100 ultrahigh-strength steel-additive manufactured builds. Electron backscattered diffraction (EBSD) revealed similar as-deposited grain sizes between the two AM processes at approximately 24 μm and 17 μm for the L-DED and AFSD samples, respectively. The strain hardening rate, θ, revealed little change in the overall hardening observed in the L-DED and AFSD materials, with a consistent hardening in the quasi-static samples and three identifiable regions in that of the high-rate tested materials. The L-DED deposited materials displayed average ultimate tensile strength values of 1835 and 2902 MPa for the 0.001 s−1 and 2500 s−1 strain rates, respectively and the AFSD deposited materials displayed ultimate tensile strength values of 1928 and 3080 MPa for the 0.001 s−1 and 2500 s−1 strain rates, respectively. Overall, the strength for both processes displayed a positive strain rate sensitivity, with increases in strength of ~1000 MPa for both processes. Fractography revealed significant solidification voids in the laser DED material and poor layer adhesion in the AFSD material.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call