Abstract
The hot deformation behavior of a γ′-hardened nickel-based superalloy was investigated by means of isothermal compression tests in the temperature range of 1010–1210°C with a strain rate of 0.1s−1. The electron backscatter diffraction (EBSD) technique and transmission electron microscope (TEM) were employed to investigate the effect of deformation temperature and strain on the microstructure evolution and nucleation mechanisms of dynamic recrystallization (DRX). Microstructure observations revealed that the size and volume fraction of DRX grains increased with the increasing temperature. A power exponent relationship was obtained between the stable DRX grain size and the peak stress. Additionally, it was found that the effect of CDRX characterized by progressive subgrain rotation became weaker with the increasing deformation temperature, and DDRX was the operating nucleation mechanism of DRX at higher deformation temperature. On the other hand, the effect of DDRX became stronger with the increasing strain, and CDRX can only be considered as an assistant nucleation mechanism of DRX at the later stage of deformation for the alloy deformed at 1160°C. Nucleation of DRX can also be activated by the twinning formation. Hence, particular attention was also paid to the evolution of twin boundaries during hot deformation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.