Abstract
Deforming nickel base superalloys under the γ′ solvus retards dynamic recrystallisation (DRX) by hampering grain boundary motion; this is an efficient way of refining grain size during forging and other hot working processes. A previously proposed model for describing the kinetics of DRX in nickel alloys is here further developed to account for the influence of γ′ intermetallics, allowing predicting microstructural evolution during subsolvus deformation. The model incorporates alloy composition and initial grain size, as well as temperature and strain rate. It is calibrated with data for both supersolvus and subsolvus deformation. Plotting the calculated steady-state grain size as a function of the strain necessary to complete DRX allows visualising both processing and compositional trends, which are relevant to materials engineering and can be used for design. It is shown that efficient grain refinement cannot be achieved with a limited amount of strain if process or alloy optimisation alone is performed. Instead, it appears that this may only be reached by joint design of the forming process (strain rate and temperature) and composition.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.