Abstract
The modulus build-up and relative density evolution during the reactive foaming of four standard polyurethane formulations was monitored in-situ by Dynamic Mechanical Analysis (DMA) with a customised set-up in parallel plate geometry. The modulus increased from 0.01 MPa in the first minutes to over 1.2 MPa within 20 min. The set-up also enabled the recording of vitrification followed by curing times. These typically occur within 3 min of each other. The results of DMA are corroborated by measurements of the reaction kinetics with Infrared Spectroscopy. This goes to show that the modulus remains nearly unchanged during the stage of swiftest isocyanate conversion, while the point of gel conversion is accompanied by their increase.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.