Abstract

Time-of-flight experiments were carried out to determine the drift mobility μ of charge carriers in a-Se 1- x Te x /Se double-layer Xerographic photoreceptors. The addition of tellurium to amorphous selenium (a-Se) in the range 0–10 wt.% progressively decreases both hole and electron drift mobilities in the charge generation layer of these photoreceptors. For tellurium concentrations greater than about 10 wt.% the electron drift mobility μ e decreases further while the hole drift mobility μ h gradually increases. These results are interpreted in terms of tellurium-induced shallow traps.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.