The composites of silica and poly (vinyl alcohol) (PVA) were prepared by sol-gel process. The composites containing more than 50wt% of PVA could be drawn in water at 50°C. The maximum draw ratio of the composites containing 50 and 80wt% of PVA were about 2.5 and 5.5, respectively. The porous silica gels were obtained by calcination of these composites at 600°C for 6 h. The obtained silica gels showed large specific surface area (700 to 950m2/g) and had micropores and mesopores of diameters of less than 10nm. The average pore size and the pore volume could be changed by drawing the composites before calcination.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.