Abstract

Hybrid Laser-Arc Welding (HLAW) technique is an enabler for the next generation high efficiency we lding, bu t in dustrial ad option ha s be en li mited du e to pr ocess complexity. Previously documented challenges with root cracks posed by incomplete penetration were significant; h owever, t his w ork p resents s uccessful w eld s amples p repared f rom S 690QL steel welded from two sides with a 16 kW disc laser. Weld travel speeds below 500 mm/min and weld line energies between 1.7 and 1.9 kJ/mm gave sound weld samples, evaluated for yield strength, elongation, hardness and Charpy-V toughness according to DS/EN ISO 10025-6:2004+A1. The results shown here indicate a significant i ncrease i n t he overall e fficiency of but t wel ds in high strength steels and further cement the HLAW process for high strength steels. It is shown that the consecutive nature of the weld procedure led to non-negligible interpass temperatures for the second weld.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.