Abstract

A spheroidal Al3(Zr,Sc) precipitate with a double-shell structure, comprising a Sc-enriched core enveloped by a Zr-enriched inner shell and a Sc-enriched outer shell (∼9 nm in thickness), appears in an Al–0.2Zr–0.1Sc alloy cable after thermomechanical treatment. The average diameter of the spheroidal Al3(Zr,Sc) precipitate is approximately 80 nm. The double-shelled Al3(Zr,Sc) precipitate presents three different interfaces and is semi-coherent with the Al matrix. Atom probe tomography (APT) analyses further show that the outer shell of Al3(Zr,Sc) precipitate is Sc element enrichment. The electrical conductivity of Al–0.2Zr–0.1Sc alloy cable increases by 6.5 MS/m within the aging time from 0.2 to 100 h at 350 °C, with double-shelled Al3(Zr,Sc) precipitate.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.