AbstractDose rate effects are important in thermoluminescent (TL) dosimeter applications because a certain absorbed dose given at different dose rates may result in a different TL yield. The present work reports about the dose rate effects on TL glow curves and kinetics properties of microwave plasma assisted chemical vapor deposition (MWCVD) diamond films grown on (100) silicon. The diamond films were exposed to γ radiation at 20.67, 43.4 and 81.11 Gy min–1 dose rates in the range of 0.05–10 kGy. The films showed a linear dose behavior up to 2 kGy and reached saturation for higher doses. The TL intensity varied as a function of dose rate and the samples had a maximum TL response for relatively lower dose rates. A single first order kinetics TL peak was typical for low doses while at higher doses two first order kinetics peaks were necessary to fit the glow curves. The results indicate that dose rate effects may be significant in dosimetric applications of MWCVD diamond. (© 2007 WILEY‐VCH Verlag GmbH & Co. KGaA, Weinheim)
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.