In this paper,Zinc oxide was dopped by various concentrations (5,10,15,20,25) % wt, silicon oxide The mixture was deposited on glass substrate by laser pulse deposition at room temperature to obtain (Zn2SiO4) thin films .The optical properties of thin films prepared on spectral absorption and transmission recording were studied at the wavelength range (200- 1100) nm. Some of the optical constants, including absorptance, transmission, absorption coefficient, and energy gap are calculated before and after annealing at (400 ̊C) for (1 hr). Absorptance values and absorption coefficient increase after doping and transmission and energy gap decreases after the doping. Absorbance values and absorption coefficient decreases after annealing and transmission and energy gap increase after the annealing .
 
 http://dx.doi.org/10.25130/tjps.24.2019.015

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.