A series of Hf: Nd: LiNbO3 crystals with various [Li]/[Nb] ratios ([Li]/[Nb] = 0.94, 1.05, 1.20, 1.38) in the melt were grown by conventional Czochralski technique. The distribution coefficients of Hf4+ and Nd3+ ions were recorded by an inductively coupled plasma-atomic emission spectrometer (ICP-AES). The effective distribution coefficient of Hf4+ is reduced and that of Nd3+ is increased with the increase of [Li]/[Nb] ratio in the melts. In all cases, the effective distribution coefficients is less than 1. The IR transmission spectroscopy of the Hf: Nd: LiNbO3 crystals were measured, getting the results that Hf: Yb: Ho: LiNbO3 crystals with 1.05 [Li]/[Nb] ratios was the stoichiometric. The optical damage resistance ability of Hf:Nd:LiNbO3 crystals were studied by light-induced scattering exposure energy flux threshold method and it increases with the increasing of [Li]/[Nb] ratios. When the [Li]/[Nb] ratio is 1.38 in the melt (the sample 4#), the exposure energy achieves 687.35 J/cm2, approximately 441 folds than that of the sample 1# ([Li]/[Nb] = 0.94) in magnitude.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call