The dissolution of MgO in CaO–“FeO”–CaF2–SiO2 slags has been studied in the temperature range 1573°–1673° K under static conditions. The concentration profiles of Mg in the product Mg1‐xFexO solid‐solution layer as well as slag were determined by EDS analysis. From this, the diffusivities of MgO in the slag and the. interdiffusivities in solid solution were estimated. The dissolution of MgO in CaO–“FeO”–CaF2–SiO2 slags increased with CaF2 content.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.