Abstract

New concepts of surface modifications aimed at the enhancement of alkali resistance of basalt fibres require research work on chemical composition of interacting surface layers as well as knowledge about fundamental processes of basaltic glass dissolution. Therefore, two model basalt fibres manufactured out of subalkaline and alkaline rock material were leached in NaOH solution at a temperature of 80°C for up to 11 days. The formation of a corrosion shell was observed in both cases and was analyzed by SEM/EDX. The model fibres out of subalkaline rocks show dissolution kinetic, which is two-staged, whereas the more alkaline fibre reflects a linear one. The complex composition of basalt fibre is detected by EDX and XPS. The surface of basalt fibres is rich in Si and Al. XPS high resolution spectra provide information on oxidation state of iron.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.