Abstract
Due to higher gravimetric and volumetric energy density than other battery technologies, Lithium-ion batteries (LIBs) have assumed an important role as portable energy systems to power electronic devices such as mobiles and laptops. However, implementation of LIBs to power automotive vehicles are limited due to their high cost, low cycle life and capacity loss at high discharge rates. For successful commercialization of electric- (EVs) and hybrid-electric (HEVs) vehicles, battery technology in terms of novel electrode materials, electrolytes and fabrication techniques needs to be further developed so that it is able to deliver better discharge capacity with improved capacity retention and cycle life. LiMn2O4 (LMO) has been used as a promising cathode material in battery systems to power EVs and HEVs due to its abundance, low cost, environmentally benign nature, minimum safety and thermal runaway issues1-3. Along with these exceptional advantages, LMO suffers from poor rate capability and cycling stability due to the imperative manganese (Mn2+) dissolution through disproportionation reaction (2Mn3+=Mn2++Mn4+), structural changes and electrolyte decomposition which act as hindrance to high power applications4-5. Research has been directed towards elucidating novel avenues to improve the cycling performance of LMO cathode for better capacity retention through investigating its electrochemical performance experimentally as well numerically3-7. However, a comprehensive numerical analysis that imitates experimental measurements towards an improved understanding of LMO degradation is missing in the literature. Consequently, galvanostatic charge/discharge, cyclic voltammetry (CV), electrochemical impedance spectroscopy (EIS), galvanostatic intermittent titration technique (GITT) and potentiostatic intermittent titration technique (PITT) has been employed in this work to quantify the performance of LMO half-cell (against Li foil anode). This experimental data has been used as an input to the numerical model to explain the phenomenon of degradation caused by manganese dissolution. Figure 1 (a) shows the experimentally and numerically obtained capacity derived from cycling two 2016 LMO coin cells at 1C rate for the first 100 cycles. The experimental and simulated results are in good agreement which indicates that capacity decreases gradually as cycle number increases. This loss in capacity, which we regard as having been caused by Mn2+ dissolution in electrolyte, induces a reduction in volume fraction of solid matrix of LMO cathode. Figure 1 (b) shows the variation of cell potential with discharge capacity for the 1st and 100th cycles, which also indicates 16.5% loss in discharge capacity due to reduction in volume fraction of solid matrix. Through this study, the rate of dissolution and loss in cyclic lithium with cycling can be quantified, and could be applied to develop novel methods of synthesis of LMO for better cycling performance and capacity retention. References M. Rashid and A. Gupta, “Mathematical model for combined effect of SEI formation and gas evolution in li-ion batteries”, ECS Electrochem. Lett., 3, A95 (2014).M. Rashid, A. Gupta, “Effect of relaxation periods over cycling performance of a li-ion battery”, J. Electrochem. Soc., 162, A3145 (2015).H. Wang, F. Lai, Y. Li, X. Zhang, and Y. Huang, “Excellent stability of spinel LiMn2O4 based cathode materials for lithium-ion batteries”, Electrochim. Acta, 177, 290 (2015).L. Cai, Y. Dai, M. Nicholson, R. E. White, K. Jagannathan, and G. Bhatia, “Life modeling of a lithium ion cell with a spinel-based cathode”, J. Power Sources, 221, 191 (2012).J. Park, J. H. Seo, G. Plett, W. Lu and A. M. Sastry, “Numerical simulation of the effect of the dissolution of LiMn2O4 particles on li-ion battery performance”, Electrochem. Solid State Lett., 14, A14 (2011).C.-H. Lu and S.-W. Lin, “Dissolution kinetics of spinel lithium manganate and its relation to capacity fading in lithium ion batteries”, J. Mat. Res., 17, 1476 (2002).Z. Zhang, T. Zeng, Y. Lai, M. Jia, and J. Li, “A comparative study of different binders and their effects on electrochemical properties of LiMn2O4 cathode in lithium ion batteries”, J. Power Sources, 247, 1 (2014). Figure 1
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have