Dissolution and reaction both play important roles in the interaction between Au studs and PbSn solders. The kinetics of interfacial reaction in this system has been studied by measuring the rate of Au consumption and growth rate of the AuSn intermetallic compound (IMC) layer at temperatures from 190 °C through 260 °C. Different AuSn compounds are identified at different isothermal bonding temperatures in accordance with the Au/Pb/Sn ternary phase diagram. The rates of Au consumption and AuSn layer growth can be shown to obey a time-based power-law relationship. The rate of Au consumption into molten eutectic PbSn solder is non-parabolic with a time exponent varying from 0.276 to 0.575. The Au consumption is faster than the growth of the AuSn layers because Au dissolves rapidly into molten solder even with the formation of intermetallic layers.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.