Abstract

ABSTRACTLap joints of an upper Al alloy (1.0-mm-thick A5052) and lower hot dip galvanized steel (1.2-mm-thick GI steel) were welded by a novel spot welding process for dissimilar metal lap joints using a new tool with the tip made of spherical ceramics, i.e. ‘Friction Anchor Welding.’ As a result, the rotating tool was plunged only to 1.3–1.4 mm from the Al alloy surface, and accordingly, a steel projection was not formed in the Al alloy sheet. Further, the Al alloy near the rotating tool was removed. However, near this removed area, the Zn layer on the GI steel melted and was removed by friction heat, and consequently, the GI steel and the Al alloy were welded. Thus, the tensile shear strength reached about 2.6 kN/point.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.