Abstract

Investigations of the influence of dispersion of feedstock on the basis of clay of the Buguruslan deposit and drill cuttings from the facilities of PJSC «Orenburgneft» have been carried out, it is revealed that as the grinding time increases, the content of clay and dust particles increases. Intensive sintering of the samples between 1000 °C and 1100 °C has been established, which is confirmed by the compaction of the samples and the decrease in the water absorption of the ceramic masses. Minimal water absorption, within 2.35%, showed a sample of 3-hour grinding, and a sample of a 2-hour grinding of 8.34%. As a result of the study of dispersion of the charge on the basis of clay raw materials and drill cuttings, it was found that by subjecting the original composition to additional processing, within 2 hours, the physical and mechanical properties of ceramic bricks can be improved.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.