Abstract

Implantation of silicon ions with an energy of 100 keV at a dose of 1 × 1017 cm−2 into n-type floatzone Si does not lead to the formation of an amorphous layer. Subsequent annealing in a chlorine-containing atmosphere at 1100°C gives rise to dislocation-related luminescence. The intensity of the dominant D1 line peaked at a wavelength of ∼1.54 μm grows as the annealing time is increased from 15 to 60 min.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.