The present study investigates the role of titanium in grain refinement of Mg–3Al and Mg–9Al alloys. Minor amount of Ti addition (<1 wt% of Al–Ti master alloy) brings about grain refinement in both Mg–3Al and Mg–9Al alloys. Ultrasonic treatment further improves the grain size reduction in Ti added Mg–Al alloys. The average grain size of Mg–Al alloys are reduced by 20–30 % from the non-refined alloy by the addition of 1 wt% of Al–Ti master alloy and ultrasonic treatment further enhances the grain refinement by 10–20 %. In addition, ultrasonic treatment transforms the network type β-Mg17Al12 phase into fine discontinuous precipitates in Ti containing Mg–9Al alloys. The mechanism of grain refinement in ultrasonic treated Ti containing Mg–Al alloy is discussed in terms of solute and heterogeneous nucleation perspective.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.