Patterned self-assembled monolayers of functionalised alkane thiols were prepared on gold substrates, using UV-photolithography. Two alkane thiols, 11-mercaptoundecanoic acid (MUA) and a fluorinated decane thiol (FDT, CF 3(CF 2) 7CH 2CH 2SH) were used to fabricate chemically structured surfaces which served as templates for zinc oxide (ZnO) crystallisation. When these patterns, containing high (MUA) and low (FDT) surface energy regions were exposed to a 10 mM zinc nitrate crystallising solution, nucleation occurred selectively on the low energy regions. After 90 min, hexagonal prisms had grown upright on these areas. The crystal growth is uniform with a crystal length of about 1 μm and a diameter between 50 and 100 nm. We attribute the selective growth to a combination of crystallographic frustration of the zinc ions on the high energy regions and an accumulation of hydroxide ions on the low energy regions.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.