High purity nickel powder (99.5% Ni) was prepared by direct hydrogen reduction of commercial NiO powder in an acidic slurry in an autoclave with a yield of approximately 100% at 250 °C, initial pH 5.4 and 300 psi partial hydrogen pressure. It was found that the initial pH of the solution and the addition of NiSO 4 play critical roles in the NiO/Ni powder conversion process. They provide an adequate acidic media and a source of SO 4 2 − counter ions for dissolving NiO into Ni 2+ ions, while the subsequent reduction of Ni 2+ ions to metallic nickel proceeds.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.