Abstract

Chromite and laterite ores from local sources were smelted in a vertical tube furnace with activated carbon as reducing agent at 1400°C to 1550°C using graphite crucible under argon atmosphere. It is shown that the grade and composition of the ore are the main factors determining the feasibility of smelting a mixture of chromite and laterite ores to produce a Fe-Ni-Cr crude alloy. The high recovery of iron and nickel in the alloy indicates the highly reducing condition prevailing in the smelting reduction experiments. It is also shown that the solubility of Ni in the slag increases with Ni concentration in the alloy and the FeO concentration in the slag. The chromium content of the slag increases with increasing iron content of the slag.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.