The application of selective ozonolysis together with high-resolution g.p.c. was performed to determine the crystalline stem lengths, in monomer units, of chain-folded lamellar crystals for trans and cis polyisoprene and polybutadiene. The trans polymer crystals were crystallized at −20°C in hexane directly from the dissolution temperature of 60°C, while the cis polymer crystals were crystallized by the same method at −70°C. The stem lengths of the trans- and cis-1,4-polyisoprene crystals were found to be 11 and 10 monomer units, respectively. Those for trans- and cis-1,4-polybutadiene crystals were found to be 12 and 13 monomer units, respectively.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.