Abstract
Magnesium-substituted hydroxyapatite coatings have been deposited on magnesium alloy for biomedical applications by sol–gel technology. The Ca(10−x)Mgx(PO4)6(OH)2coatings obtained, with magnesium contents up to x = 1.5, show dense and compact and with visible cracks. The results of Hydrogen (H2) evolution testing in Hank’s solution show that magnesium-substituted hydroxyapatite coatings can improve the corrosion resistance of magnesium alloy.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of Biomimetics, Biomaterials and Biomedical Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.