Abstract

We report on an efficient diode-end-pumped polycrystalline Yb:Y2O3 ceramic laser. Continuous-wave output power of 4.2 W at 1078 nm was obtained under pump power of 19.5 W. The corresponding slope efficiency was 29%. The beam quality factor (M2) at full pump power was measured to be 1.63. The threshold wavelengths of the laser at various output couplings were also investigated. It was found that the threshold wavelengths shifted approximately 5 nm when the reflectivity of the output coupler changed from 90% to 99.9%, as caused by the strong reabsorption effect in the ceramic sample.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.