Post-heat treatment experiments were carried out for complete dimensional stabilization of thermally compressed wood (Pinus koraiensis). An absorption test was carried out to evaluate the dimensional stability. The specific gravity increased from 0.43 to 0.79 by thermal compression at a compression ratio of 50% thickness. Through the post-heat treatment of compressed wood, the water absorption and thickness swelling decreased with increasing the heat treatment temperature and time. In the case of the thickness recovery rate, when the heat treatment was performed for 24 hours at 120 °C, 140 °C and 160 °C, the thickness recovery was less than 1%. Therefore, it can be confirmed that the method of dimensional stabilization method of the thermal compression wood can be carried out very effectively through post heat treatment process.