Abstract

We have measured length change vs time for several low thermal expansion materials maintained in evacuated environments at constant temperature (near 300 K). Materials were two types of fused silica, Cer-Vit, ULE, Zerodur, Invar, and super Invar. ΔL/L was measured over a period of 170 days to a precision of two to three parts in 109. In addition, we have measured time-dependent changes in optical contact interfaces and have placed an upper limit on drift of optical phase shift on reflection from multilayer dielectric coatings.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.