Abstract

The fiber dimension and chemical composition of Persea sp. are presented in this report. The analyses include determination of the fiber dimension (length, diameter cell wall t h ickne s s, and Runkel ratio), and chemical composition. (cellulose, lignin, pentosan, ash, extractives, and solubility in one percent sodium hydroxide solution). The study reveals that the average fiber length is 1105.36 µ , diameter 19. 09 µ , cell wall thickness 2,36 µ and Runkel ratio 0.37. The cellulose content amounts to 45.46 percent, lignin 23.71 per cent, pentosan 19.67 percent and ash 1.27 percent. The solubility in cold water ; was found to be 5.43 percent; in hot water 5.55 percent, in alcohol benzene 1:2 ratio, 4.02 percent and in one per cent sodiumhydroxide solution 11.36 percent. Based on the fiber dimension and the chemical composition, it was found that Persea wood is suitable for producing good quality paper.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.