Abstract

Y2W3O12 exhibits negative thermal expansion along the three crystallographic directions due to the transverse thermal vibrations perpendicular to the Y-O-W linkage. It is highly hygroscopic and forms a trihydrate structure at room temperature. Dilatometric studies of Y2W3O12 show large thermal expansion hysteresis due to large grain size and a large initial positive thermal expansion due to the removal of water molecules. Al2O3 has been added to Y2W3O12 upto 10 wt% in an attempt to overcome the hygroscopicity and reduce the particle size and thereby the thermal expansion hysteresis. Thermo gravimetric, dilatometric and electron microscopic studies are presented to support these observations.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.