Abstract
The diffusion of water and benzene has been followed by DSC using the thermoporosimetry (TPM) approach. The diffusion of water has been observed during the drying of a water impregnated mesoporous silica gel at 40 degrees C under dry air. It was found that the confinement affects the evaporation rate of water. The diffusion of benzene has been observed during the drying and the swelling of a cross linked PDMS sample. The mesh size distributions (MSD) of the elastomer, during swelling and drying, have been calculated at various times using the TPM formalism. Extrapolating the mean mesh size of the polymeric network, it was found that the dry polymer has an average mesh of about 2.5 nm.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.