The glass-forming tendency and specific heat in ice cold water-quenched Ge1−xSnxSe2.5 glassy alloys with 0<x<0.6 were investigated by means of differential scanning calorimetry. The heat of fusion ΔH f, the heat ΔH c associated with the crystallization of an amorphous phase and the glass transition temperatureT g were deduced from the DSC curves. The composition dependence of glass forming ability,T g and crystallization behavior has been discussed.