Abstract
The high temperature phase relations (20°C) of LiH 2PO 4, NaH 2PO 4, KH 2PO 4, RbH 2PO 4, CsH 2PO 4, NH 4H 2PO 4, KH 2AsO 4, RbH 2AsO 4, CsH 2AsO 4 and NH 4H 2AsO 4 have been studied. All materials decompose at higher temperatures. Solid—solid transitions are studied when present and transition temperatures, transition enthalpies, decomposition temperatures, decomposition enthalpies and decomposition products are discussed.