ABSTRACT Differential scanning calorimetry (DSC) was employed to detect high oleic sunflower oil (HOSo) as an adulterant in extra‐virgin olive oil (EVOo) by means of cooling and heating thermograms. Addition of HOSo did not significantly alter cooling profiles of EVOo except for onset temperature of crystallization, which was significantly shifted toward lower temperature at 40% of adulterant addition. At the same percentage of adulteration, the heating profile of EVOo was significantly changed as the major endotherm broadened and the minor event became smaller and less evident. Cooling thermograms of pure oils and their admixtures were deconvoluted into three constituent exothermic peaks in an attempt to detect addition of HOSo at levels lower than 40%. Thermal properties of the two lower‐temperature exotherms (area percentage, offset temperature and range of transition) were significantly changed at≥20% of HOSo substitution, suggesting that DSC can be employed to detect this oil as an EVOo adulterant.PRACTICAL APPLICATIONSAdulteration of extra‐virgin olive oil (EVOo) with cheaper oils from other vegetable sources or seeds, as well as with lower quality olive oils, is a serious concern for oil suppliers and consumers and requires the use of new analytical techniques for their detection. Differential scanning calorimetry (DSC) exhibits some advantages over the classical analytical methods as it does not require sample preparation and use of solvents, thus resulting in a reduced environmental impact. Results suggested that its application to the detection of EVOo adulteration with high oleic sunflower oil, a vegetable oil largely employed for this type of fraud, is promising with the support of the deconvolution analysis of cooling thermograms.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.