Abstract

Differential voltage analysis (DVA) is a conventional approach for estimating capacity degradation in batteries. During charging, a graphite electrode goes through several phase transitions observed as plateaus in the voltage response. The transitions between these plateaus emerge as observable peaks in the differential voltage. The DVA method utilizes these peaks for estimating cell degradation. Unfortunately, at higher C-rates (above C/2) the peaks flatten and become unobservable. In this work, we show that, unlike the differential voltage, the peaks in the 2nd derivative of the expansion with respect to capacity remain observable up to 1C and thus make possible diagnostic algorithms at these charging rates. To understand why that is the case, we have developed an electrochemical and expansion model suitable for model-based estimation. In particular, we demonstrate that the single particle modeling methodology is not able to capture the peak smoothing effect, therefore a multi-particle approach for the graphite electrode is needed. Additionally, model parameters are identified using experimental data from a graphite/NMC pouch cell. The proposed model produces an excellent fit for the observed electric and mechanical swelling response of the cells and could enable physics-based data-driven degradation studies at practical charging rates.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.