Abstract

Dielectric Ba0.6Sr0.4TiO3 films doped with different weight percentages of TiO2 were deposited by pulsed-laser deposition. The dielectric constant, dielectric loss, and the dielectric tunability of the films were found to be a strong function of the weight ratio of TiO2/Ba0.6Sr0.4TiO3. Compared to the pure Ba0.6Sr0.4TiO3, the TiO2-doped Ba0.6Sr0.4TiO3 exhibits lower dielectric loss while maintaining a significantly adjustable dielectric constant and desirable capacitance tunability. The change of the dielectric properties of TiO2-doped Ba0.6Sr0.4TiO3 films is closely related to the change in microstructure of the films as revealed by transmission electron microscopy.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.