Dielectric properties and tunability of Ba0.60Sr0.40TiO3 (BST) and BaZr0.25Ti0.75O3 (BZT) thick films and bulk ceramics have been investigated as a function of temperature (90 K - 320 K) in the kHz region. Thick films show compared to bulk ceramics low permittivity and a very broad ferroelectric phase transition which leads to low temperature dependence of tunability. Tunability of 30% can be achieved with an external field of 2 kV/mm. Measurements in the microwave region adumbrate that the dielectric losses of BZT are about three times higher than that of BST thick films.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.