Abstract

(1-x)Ba(Fe0.5Nb0.5)O3 -xBiYbO3 (BFN-xBY) ceramics were prepared by a conventional solid-state reaction method. The dielectric properties and relaxation behavior of BFN-xBY ceramics were analyzed according to dielectric and impedance spectroscopy. Dielectric permittivity of the ceramics increases with increasing temperature below 500 K then remains unchanged up to 700 K, while corresponding loss factor decreases with the increase of temperature below 500 K then increase slowly. Defect compensation mechanism of this system was analyzed in detail. The giant dielectric behavior of the ceramics arises from the internal barrier layer capacitor (IBLC) effect. Polarization effect at insulating grain boundaries between semiconducting grains accompanied by a strong Maxwell-Wagner (MW) relaxation mode. The characteristic of grain boundaries was revealed using impedance spectroscope and the universal dielectric response law.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.