Abstract

The temperature dependences of the dielectric constant and dielectric hysteresis loops in ceramic samples of (1 − x)SrTiO3−xKNbO3 and (1 − x)SrTiO3−xKTaO3 (0 ≤ x ≤ 0.3) solid solutions prepared using different heat treatments have been investigated. Phase diagrams of the studied solid solutions have been constructed in the T-x coordinates. It has been shown that, after quenching of samples (spontaneous cooling at room temperature after long-term heating at the sintering temperature of the ceramic samples), the temperature of the induced phase transition increases because of the weakening of random electric fields associated with nonisovalent impurities due to their “frozen” nonequilibrium redistribution. For small concentrations x, strong dielectric relaxation is observed in the temperature range of 150–250 K. A model of relaxing centers, which is based on the local charge compensation of heterovalent impurities, has been proposed.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.