Abstract

AbstractIn this work lead‐free 0.75SrTiO3‐0.25BiTiO3 ceramics have been investigated in broad frequency range. Obtained results showed pronounced dispersion below room temperature typical for the dipolar glasses. The calculated relaxation time distribution function broadens toward longest relaxation times part on cooling. The obtained most probable relaxation time diverges according to the Vogel‐Fulcher relationship with the following parameters: dipole activation energy EA=2123 K, glassy state temperature T0=52.7 K, shortest relaxation time, referring to dipole relaxations at very high temperatures, τ0=2.1·10–14 s. (© 2009 WILEY‐VCH Verlag GmbH & Co. KGaA, Weinheim)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.