The dielectric constants and dielectric loss values of BeAl2O4 (chrysoberyl), MgAl2O4 (spinel), Be2SiO4 (phenacite), and Mg2SiO4 (forsterite) were measured at 1 MHz using a two-terminal method and empirically determined edge corrections. The results are: chrysoberyl, κ′ a =9.436, κ′ b =9.071, κ′ c =8.269; spinel, κ′ a =8.18; phenacite, κ′ a =6.28, κ′ c =6.06; and forsterite, κ′ a =6.867, κ′ b =7.392, κ′ c =6.739. The agreement between measured dielectric polarizabilities as determined from the Clausius-Mosotti equation and those calculated from the sum of oxide polarizabilities according to αD(M2M′X4) = 2αD(MX)+αD(M′X2) is ~ 1.0%.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.