Abstract

We investigate the dielectric and ferroelectric properties of Sr1−xBixTi1−xFexO3 solid solutions (x = 0, 0.05, 0.1, 0.15 and 0.2) together with their structures. Through the analysis of Rietveld refinement of powder x-ray diffraction, a cubic structure in space group Pm3̄m is determined for all the compositions. An obvious dielectric relaxation peak differing from SrTiO3 is observed in the present ceramics. The peak temperature Tm increases with increasing x, and it approaches room temperature at x = 0.2. The Vogel—Fulcher law and Curie—Weiss law fittings further confirm the relaxor ferroelectricity in the present ceramics.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.