Porous barium calcium zirconate titanate 0.5Ba(Ca0.8Zr0.2)O3-0.5(Ba0.7Ca0.3)TiO3 (BCZT) lead-free ferroelectric ceramics were fabricated via a burnt polymer spheres (BURPS) technique by introducing corn starch as the pore-forming agent. The effect of porosity on the microstructure, dielectric, and piezoelectric properties of the porous materials were investigated. An increase in porosity volume fraction from 10% to 25% resulted in an increase in the hydrostatic charge coefficient (dh), which was 140 to 560% higher than that of the dense BCZT material. An increase in porosity fraction from 10% to 25% also lead to a decrease in relative permittivity that was 16.7% to 60.4% lower than the dense material. These two changes in properties provided a significant enhancement of the hydrostatic figure of merit (dh∙gh) for the porous ceramic; for example the dh∙gh of the 25 vol.% porous BCZT ceramic was 158 times more than the dense ceramic and demonstrates the potential of porous lead-free ferroelectrics for piezoelectric transducer devices. Reasons for the significant enhancement in piezoelectric performance of the porous ceramics are discussed.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call